| Test Items | ASTM | Unit | Value | ||||||
| Density | D1505 | g/cm³ | 0.96 | ||||||
| Melt Index | D1238 | g/10min | 0.5 | ||||||
| HLMI | D1238 | g/10min | --- | ||||||
| Condition A, F50(100% Igepal) | D1693 | h | >500 | ||||||
| Condition B, F50(100% Igepal) | D1693 | h | --- | ||||||
| Tensile Yield Strength,50mm/min | D638TypeIV | Mpa | 26 | ||||||
| Elongation at Break,50mm/min | D638TypeIV | % | >300 | ||||||
| Brittleness Temperature | D746 | ℃ | <-40 | ||||||
| Flexural Modulus, Tangent | D790 | Mpa | 950 | ||||||
| Shore D Hardness | D2240 | - | 65 | ||||||

![]()

Feature
High abrasion and impact resistance
UV Resistant
Easily machined for Engineering Use
Almost completely inert to chemical attacks
Zero coefficient of friction
Non-caking & sticking
Good electrical properties
Performs very well in colder temperature applications
Maximum temperature: 180°F
Water absorption < 0.01%